Using liquid silicone in winter is a complete contrast to summer. Summer is a chaotic race against time, while winter is a test of patience and temperature control. The core challenges in winter are: a dramatic increase in viscosity due to low temperatures, extremely slow curing, and the easily overlooked problems of condensation and crystallization traps.
When using liquid silicone in winter, pay close attention to the following key precautions to ensure operational safety and product performance:
Temperature Control: The Key to Curing and Handling
Curing Temperature Requirements: Silicone curing is temperature-sensitive. Low winter temperatures (<10℃) may lead to incomplete curing or significantly prolonged curing time. The recommended operating temperature is 20-25℃. Addition-type silicone can be cured more quickly by heating, such as approximately 30 minutes at 80℃ or 15 minutes at 120℃. Condensation-type silicone should avoid a hardener ratio exceeding 100:4, otherwise it will damage the molecular structure and lead to performance degradation.
Avoid Extreme Low Temperatures: If the ambient temperature is <5℃, the silicone may not cure at all; refrigerated silicone should be brought to room temperature before use to prevent a sudden increase in viscosity from affecting mixing.
Storage Conditions: Extending Shelf Life and Enhancing Stability
Ideal Storage Environment: Cool, dry, and well-ventilated place, temperature controlled between 5-25℃, away from high temperatures, humidity, fire sources, and chemicals. Unopened food-grade silicone typically has a shelf life of 12-18 months. Once opened, it should be used within 3-6 months. Components A and B must be sealed separately to avoid mixing and inactivation.
Expired Product Handling: Expired silicone should not be used if it shows signs of separation, clumping, odor, or abnormal curing. If there is no obvious deterioration, a small batch can be tested for curing effect, but expired products are not recommended for food/baby contact scenarios.
Special Issues and Solutions
Slow/Non-Curing: Increase ambient temperature and humidity; check the hardener ratio and mixing uniformity. If caused by low temperature, try extending the curing time or using baking to accelerate the process.
Surface Defects: Wrinkling, whitening, etc., may be due to excessively fast surface drying and uneven inner layer curing. This can be improved by creating a constant temperature and high humidity environment, covering to reduce airflow, or using a slower-drying adhesive.
Contamination and Impurities: Molds/pipes must be clean and free of grease. Operating tools should be replaced regularly to prevent dust and grease from contaminating the silicone compound. Color pastes must be selected from compatible products and thoroughly mixed to prevent uneven coloring.
These measures effectively address the impact of low winter temperatures on liquid silicone, ensuring curing results, product performance, and operational safety.