logo
Home >

Latest company case about Shenzhen Hanast New Material co.,LTD Certifications

Why is the potting still tacky after 24 hours?

2025-06-17

Latest company case about Why is the potting still tacky after 24 hours?

Incorrect mix ratio, low temperature, or expired product—verify process and materials.