Home > Products >
High Flow Single Component Thermal Gel 10.0 W/mK for AI Server Optical Module Heat Dissipation

High Flow Single Component Thermal Gel 10.0 W/mK for AI Server Optical Module Heat Dissipation

Product Details:
Place of Origin: Guangdong, China
Brand Name: Hanast
Certification: RoHS 2.0 / Halogen-Free / REACH
Model Number: HN-6100PC-1
Detail Information
Place of Origin:
Guangdong, China
Brand Name:
Hanast
Certification:
RoHS 2.0 / Halogen-Free / REACH
Model Number:
HN-6100PC-1
Thermal Conductivity:
10.0 +/- 0.5 W/mK (ISO 22007-2)
Bond Line Thickness:
120 Um (ASTM D5470)
Density:
3.1 +/- 0.1 G/cm3 (ASTM D792)
Hardness After Cure:
45 +/- 10 Shore OO (ASTM D 2240)
Extrusion Rate:
>=30 G/min (30CC Tube @ 0.6 MPa)
Volume Resistivity:
>=1.0 X 10^10 Ohm.cm (ASTM D257)
Dielectric Breakdown Voltage:
>5 KV (ASTM D149)
Operating Temperature Range:
-40 To 150 C
Cure Behaviour:
Post-cure, Heat Accelerated, Stays Soft
Application Format:
Single Component Gel For Automatic Dispensing
Highlight:

High Light

Highlight:

10.0 W/mK Thermal Conductivity

,

High Flow Automated Dispensing

,

Low BLT Optical Module Cooling

Trading Information
Minimum Order Quantity:
1 Tube (30CC)
Packaging Details:
30CC syringe tube, 300ML cartridge, 20KG pail with inner liner and export carton
Delivery Time:
3-4 working days for stock items, 10-15 days for bulk orders
Payment Terms:
T/T,D/A,D/P
Supply Ability:
50 Tons per Month
Product Description

AI accelerators, 800G optical transceivers and high density networking switches push more heat through smaller contact areas than any previous generation of data centre hardware. Thermal grease pumps out of the joint within the first thousand power cycles, and gap pads leave voids on warped lids and rough housings. This post-cure single component thermal gel is built for exactly that interface: it dispenses like a paste, holds the bead where it is placed, and cures into a soft, heavily filled silicone cushion with 10.0 W/m·K thermal conductivity at a bond line of only 120 µm.

Because the material is a one-part system, there is no A/B mixing station, no pot life clock and no mixed-material scrap on the line. It extrudes at 30 g/min or more from a 30CC tube at 0.6 MPa, which keeps up with the takt time of automated dispensing cells used on optical module, switch and server assembly lines. The pink colour makes coverage easy to confirm with a single camera check before the heat sink is seated.

Product Gallery
Single component thermal gel supplied in a 30CC syringe for automated dispensing on server and optical module lines 10.0 W/mK thermal gel bead applied across an optical module heat sink before assembly Post cure thermal gel compressed to a 120 micron bond line on a server cold plate
Key Features
  • 10.0 W/m·K thermal conductivity: a high filler loading keeps junction temperatures under control on 400 W to 1000 W accelerator packages without increasing bond line thickness.
  • Low 120 µm BLT: the paste wets and thins under normal mounting pressure, so thermal resistance stays low even on lapped cold plates and vapour chambers.
  • High flow for high volume lines: extrusion of 30 g/min or more from a 30CC tube at 0.6 MPa supports jetting, time-pressure and screw pump dispensers already installed in most contract manufacturers.
  • Post-cure soft gel: after heat accelerated cure the material sits at 45 ± 10 Shore OO, absorbing CTE mismatch between silicon, copper and aluminium instead of transferring stress to the die.
  • High electrical insulation: volume resistivity of at least 1.0×1010 Ω·cm and dielectric breakdown above 5 kV allow direct contact with live components and power modules.
  • Stable from -40 to 150 °C: no pump-out, no hardening and no oil bleed through power cycling, vibration and damp heat ageing.
  • Storage stability: six months at 25 °C or below with no settling or skinning, so a 20 KG pail can be used across several production weeks.
  • Export ready compliance: RoHS 2.0, halogen-free and REACH documentation supplied with every shipment for programmes that re-export to the EU and North America.
Technical Specifications
Parameter Typical Value and Test Method
Thermal Conductivity 10.0 ± 0.5 W/m·K (ISO 22007-2)
Bond Line Thickness (BLT) 120 µm reference (ASTM D5470)
Color Pink, visual inspection friendly
Density 3.1 ± 0.1 g/cm³ (ASTM D792)
Hardness After Cure 45 ± 10 Shore OO (ASTM D 2240)
Extrusion Rate ≥30 g/min from 30CC tube at 0.6 MPa
Volume Resistivity ≥1.0×1010 Ω·cm (ASTM D257)
Dielectric Breakdown Voltage >5 kV (ASTM D149)
Operating Temperature Range -40 to 150 °C
Cure Behaviour Post-cure, heat accelerated; soft gel after cure
Shelf Life 6 months at ≤25 °C; 1 month outside storage conditions
Storage Conditions Dark place, ≤25 °C, ≤70% RH, no squeezing or direct sunlight
Compliance RoHS 2.0, halogen-free, REACH
Applications

The material is aimed at heat paths where the gap is small, the power density is high and rework is expensive. Typical uses include thermal interface between optical transceiver cages and heat sinks, GPU and CPU packages on accelerator boards, switch ASIC lids and vapour chambers, power modules inside server PSUs, and SSD controllers on densely packed storage cards. It is equally suitable for telecom remote radio units and outdoor small cell housings, where the joint must survive humidity and daily temperature swings for a decade.

Dispensing patterns are simple: a serpentine bead for large lids, a single dot for small packages, or a stencil printed pad for panel level assembly. No curing oven is required for many designs; where a cured, non-flowing cushion is preferred for transport or vertical mounting, a short heat cycle accelerates the post-cure and locks the gel in place.

High Flow Single Component Thermal Gel 10.0 W/mK for AI Server Optical Module Heat Dissipation

Who This Product Is For Factory owners and plant directors in Vietnam and Malaysia

One SKU covers optical module, switch, server and storage heat paths, so fewer materials are qualified and fewer lines need requalification when a new platform is introduced. Because there is no mixing, there is no mixing station headcount and no expired mixed batch to scrap. Capacity of about 50 tons per month supports ramp programmes in Bac Ninh, Bac Giang, Penang and Johor without a second source.

Procurement teams

Evaluation can start from a single 30CC tube, then move to 300 ML cartridges for semi-automatic cells or 20 KG pails for bulk automatic dispensing, so no drum commitment is needed during qualification. Stock items ship in three to four working days, and payment terms can follow your existing supplier workflow with T/T, D/A or D/P.

Process and manufacturing engineers

Rheology is tuned for standard dispensers: extrusion above 30 g/min at 0.6 MPa, no sag on vertical faces, no curing oven in the flow, and a bond line set by mounting force rather than by material flow. Every number in the specification table carries its test method, so incoming inspection and line trials can be reproduced in your own laboratory.

Product managers and design owners

Where a platform currently mixes grease on some boards and pads on others, one post-cure gel can replace both, cutting part numbers and BOM complexity. The 0.1 to 1.0 mm working gap covers most lid-to-heat-sink and housing interfaces, and the cured softness gives mechanical decoupling that rigid adhesives cannot offer.

Packaging and Quality Assurance

Standard packaging is a 30CC syringe tube for evaluation, a 300 ML cartridge for semi-automatic lines and a 20 KG pail for bulk automatic dispensing. Every batch is released against the properties listed above, with retain samples kept for twelve months. Certificates of analysis, RoHS 2.0, halogen-free and REACH declarations, and a full TDS are supplied with the quotation. Store the material in a dark place at 25 °C or below and 70% RH or below, keep pails upright and avoid direct sunlight or squeezing of the containers.

Frequently Asked Questions
  • Does the gel need mixing before use? No. It is a single component, ready-to-dispense material. There is no A/B ratio, no pot life and no mixed-material waste.
  • Will it flow out of a vertical gap? No. The rheology holds the bead in position on vertical and overhead surfaces, and the cured gel does not migrate during thermal cycling.
  • Is a cure step mandatory? No. Many designs run with the uncured gel compressed in place. A heat cycle is used when a non-flowing cushion is required for transport or for vertical mounting.
  • Can it be reworked? Yes. The cured material stays soft, so heat sinks can be separated mechanically and the residue removed with alcohol before reapplication.
  • What documentation is provided for export programmes? TDS, COA, RoHS 2.0, halogen-free and REACH declarations are issued with each quotation, which covers modules assembled in Vietnam or Malaysia and shipped onward to the EU and North America.
Related Products

Both grades share the same silicone chemistry, so a single qualification covers different gaps on the same line.

similar products