HN-8810A/B is a two-component, 1:1 addition-cure silicone potting compound with 1.0 ± 0.1 W/m·K thermal conductivity, UL94 V-0 flame retardancy and only 2000–3000 mPa·s mixed viscosity. The low viscosity is the key point for two-wheeler battery assembly: it flows into the narrow gaps between 18650/21700 cell holders, nickel strips, sense wires and the BMS board, then cures into a rubber-elastic block that conducts heat, insulates electrically and seals out moisture. It cures at room temperature or in 10–20 minutes at 80 °C, which fits existing e-bike, e-scooter and e-motorcycle pack lines in Southeast Asia.
1.0 W/mKThermal conductivity
UL94 V-0Flame retardancy
2000–3000mPa·s mixed viscosity
−40~+150 °CService range

HN-8810A/B two-component 1.0 W/mK silicone potting compound
What Is HN-8810A/B?
HN-8810A/B is a two-component addition-type (platinum-catalysed) thermally conductive silicone potting compound. Component A is a white liquid polysiloxane and Component B is a grey liquid polysiloxane, both at 2000–3000 mPa·s and 2.0 ± 0.02 g/cm³. Mixed 1:1 by weight they stay at 2000–3000 mPa·s, pour and self-level, then cure into a grey elastic silicone.
Because the viscosity is roughly one fifth of a typical 3 W/m·K potting grade, it reaches the bottom of a deep, densely packed battery cavity and wets the surfaces of cells, holders and busbars without leaving voids. Voids are where heat transfer and waterproofing both fail, so low viscosity directly improves the two properties battery engineers care about most.
Why Two-Wheeler Battery Packs Use This Grade
- Fills dense 18650 / 21700 arrays: low viscosity penetrates between cell holders and busbars instead of bridging across the top, so no air pockets remain under the pack.
- Heat path from cells and BMS to the aluminium case: 1.0 W/m·K pulls heat out of high-rate discharge hotspots and away from MOSFETs on the BMS board during fast charging.
- Vibration and shock protection: cured elasticity holds cells, nickel strips and sense wires in place over potholes, kerbs and rough roads.
- Waterproof and moisture-proof: full encapsulation supports IP-rated pack designs and protects against rain, washing and tropical humidity cycling.
- Flame safety: UL94 V-0 rated cured silicone reduces propagation risk in a pack that sits under the footboard or behind the leg shield.
- Production friendly: 1:1 by weight, 10–20 minute cure at 80 °C, and low mixed viscosity that works with existing dispensing and vacuum potting equipment.
Before Mixing (Component Properties)
| Property | Test Method / Condition | Unit | Component A | Component B |
| Appearance | Visual | — | White liquid | Grey liquid |
| Base Chemistry | — | — | Polysiloxane | Polysiloxane |
| Viscosity | GB/T 2794-1995 | mPa·s (cP) | 2000–3000 | 2000–3000 |
| Density | GB/T 2794-1995 | g/cm³ | 2.0 ± 0.02 | 2.0 ± 0.02 |
After Mixing (A+B)
| Property | Test Method / Condition | Unit | Value |
| Appearance | Visual | — | Grey liquid |
| Base Chemistry | — | — | Polysiloxane (silicone) |
| Mix Ratio (A:B) | By weight | — | 1:1 |
| Mixed Viscosity | GB/T 2794-1995 | mPa·s | 2000–3000 |
| Cure Time (Heat Accelerated) | 80 °C | min | 10–20 |
Cured Properties
| Property | Test Method / Condition | Unit | Value |
| Thermal Conductivity | GB/T 38712-2020 | W/m·K | 1.0 ± 0.1 |
| Volume Resistivity | GB/T 31838.2-2019 | Ω·cm | ≥ 5.0 × 1014 |
| Flame Retardant Rating | UL94 | — | V-0 |
| Operating Temperature Range | — | °C | −40 to +150 |
Recommended Curing Schedule
| Cure Option | Condition | Duration | Notes |
| Room-temperature cure | 25 °C | Refer to pot life | Full cure at ambient temperature |
| Heat-accelerated cure | 80 °C | 10–20 min | Fast cure for production lines |
Mixing and Potting Procedure
- Pre-mix separately: stir Component A and Component B thoroughly before use so settled filler is fully dispersed.
- Weigh 1:1 by weight: use a precision scale. Volume-based mixing shifts the ratio and can leave the pack tacky.
- Mix to uniform colour: hand or machine mixing is acceptable; avoid preparing very large batches by hand because fluidity drops and potting becomes difficult.
- Degas: place the mixed compound in a vacuum cabinet to remove entrapped air before pouring.
- Pot the pack: pour into the clean, dry housing and let it self-level around cells, holders and BMS; ensure the housing and mixing container are dry.
- Cure: cure at room temperature or 80 °C for 10–20 minutes. Viscosity rises over time, so finish potting within the working time and never return mixed material to the original drums.
Catalyst poisoning warning for engineers
This addition-cure (platinum) silicone will not cure if it touches organotin or tin-containing silicone rubber, sulphur or polysulphide compounds, amines, polyurethane rubber, ammonia, phosphorus compounds, organic acids, or solder flux residues. Clean substrates, tooling and containers before potting, and run a trial cure on the actual cell holder and BMS board before mass production.
For Buyers: Supply Terms
| Item | Detail |
| Minimum order quantity | 1 kg for trial; 50 kg sets (25 kg A + 25 kg B) for production |
| Price | Negotiable, volume pricing on bulk orders |
| Packaging | 25 kg iron or plastic drum per component, 50 kg per set |
| Lead time | 5–7 days |
| Payment terms | T/T, PayPal |
| Documentation | TDS, MSDS and COA with shipment |
Who This Product Is For
Factory owners
Low-viscosity potting removes the void problems that cause rework and field returns, and the 10–20 minute 80 °C cure keeps pack lines at takt time without adding ovens.
Procurement teams
1 kg trial for qualification, 50 kg sets for series production, 5–7 day lead time, and a stable 1:1 ratio that simplifies incoming inspection and drum management.
Engineers
Full uncured, mixed and cured data, GB/T and UL94 references, plus an explicit catalyst-poisoning list so the first pack does not fail on contaminated holders or flux residue.
Product managers
Matched to in-house battery programmes for e-bikes, e-scooters and e-motorcycles: 48 V, 60 V and 72 V packs, BMS encapsulation and charger modules, with waterproofing and V-0 built in.
Silicone Potting Compound: Common Buying Terms
This product family is searched under many English names. All of the queries below describe the same material, and HN-8810A/B covers each of them:
silicone potting compoundpotting siliconeaddition cure silicone pottingRTV silicone encapsulantthermal potting compoundbattery pack potting compoundBMS potting siliconetwo-component potting gluelow viscosity potting compound1:1 potting siliconewaterproof electronic encapsulantUL94 V-0 potting compound
When comparing suppliers for battery pack potting, ask four numbers: mixed viscosity, thermal conductivity, UL94 rating and the maximum single-pour depth. These decide whether the compound can fill a deep cell cavity without voids.
Product Gallery
Frequently Asked Questions
What is HN-8810A/B used for?It is a thermally conductive silicone potting compound for encapsulating battery packs, BMS boards, power modules and circuit boards, providing heat transfer, insulation, vibration support and waterproofing in one cured block.
What is the thermal conductivity?1.0 ± 0.1 W/m·K measured by GB/T 38712-2020 on the cured elastomer.
What is the mixed viscosity and why does it matter?2000–3000 mPa·s, low enough to flow between 18650/21700 cell holders and busbars in a deep pack, which prevents voids that block heat transfer and water ingress.
What is the mix ratio?1:1 by weight between Component A and Component B. Mix by weight with a precision scale, not by volume.
How fast does it cure?10–20 minutes at 80 °C for heat-accelerated production lines, or full cure at 25 °C following the pot life.
Is it flame retardant?Yes, UL94 V-0 rated, which matters for packs mounted under the footboard or behind the leg shield.
What is the operating temperature range?−40 °C to +150 °C according to the cured property data. Note that the general overview section of some TDS versions quotes a wider figure; use the cured property table for design calculations.
Is it waterproof?Yes. Complete encapsulation removes the air voids where condensation forms, supporting IP-rated battery and charger designs.
Why would the silicone fail to cure?Platinum addition cure is inhibited by tin, sulphur, amine, polyurethane, ammonia, phosphorus, organic acids and flux residues. Clean holders and boards, or trial-cure before mass production.
What is the MOQ and lead time for Southeast Asia?MOQ is 1 kg for trial and 50 kg sets for production, with 5–7 day lead time from Guangdong, China to Vietnam, Thailand, Indonesia, Malaysia and the Philippines.
Trial potting for your e-bike or e-scooter battery pack?
Send your pack drawing, cavity volume, cell format (18650 or 21700), annual output and target IP rating. We reply with grams per pack, a potting trial plan and bulk pricing within one working day.
Overall Rating
Rating Snapshot
The following is the distribution of all ratingsAll Reviews