Home > Products >
Thermally Conductive Potting Compound
>
4.0 W/mK Thermal Conductivity UL 94 V-0 Flame Retardant 1:1 Mix Ratio Thermally Conductive Potting Compound for 800V SiC Inverter Power Stack

4.0 W/mK Thermal Conductivity UL 94 V-0 Flame Retardant 1:1 Mix Ratio Thermally Conductive Potting Compound for 800V SiC Inverter Power Stack

Product Details:
Place of Origin: Guangdong, China
Brand Name: Hanast
Certification: UL 94 V-0, RoHS 2.0, ISO 9001:2015
Model Number: HN-8840A/B
Detail Information
Place of Origin:
Guangdong, China
Brand Name:
Hanast
Certification:
UL 94 V-0, RoHS 2.0, ISO 9001:2015
Model Number:
HN-8840A/B
Thermal Conductivity:
4.0 ± 0.1 W/m·K
Flame Retardancy:
UL 94 V-0
Mix Ratio:
1:1 By Weight
Mixed Viscosity:
13,000 ± 2,000 MPa·s At 25 °C
Mixed Density:
2.95 ± 0.02 G/cm³ At 25 °C
Pot Life:
60 To 180 Min At 25 °C (100 G Mix)
Cure Time Room Temperature:
4 To 8 H At 25 °C
Cure Time Heat Accelerated:
30 Min At 80 °C
Hardness:
Shore A 45 ± 8
Volume Resistivity:
≥ 1.0 × 10^14 Ω·cm
Operating Temperature:
-40 To +200 °C
Appearance:
White Liquid A / Grey Liquid B, Grey Elastomer After Cure
Curing System:
Two-component Addition Cure (platinum Catalysed)
Application Method:
Meter-mix, Static Mixer, Manual Weighing, Vacuum Degassing, Pour Potting
Key Property:
High Heat Flux, Die Level Thermal Coupling, Cast In Place
Typical Applications:
Traction Inverter, Motor Controller, SiC And IGBT Module, Double-sided Cooling Module, Power Stack, OBC, DC-DC, BMS, Battery Module, EV Charger, Energy Storage, PCS, PV Inverter, Power Supply
Packaging:
25 Kg Barrels A And B, 50 Kg A+B Kit
Shelf Life:
6 Months At 5 To 25 °C
Transport Classification:
Non-dangerous Goods
Compliance:
UL 94 V-0; RoHS 2.0
Target Market:
Southeast Asia (Vietnam, Thailand, Indonesia, Malaysia, Philippines)
Highlight:

High Light

Highlight:

High Heat Flux Potting Compound

,

800V SiC Traction Inverter Potting

,

Southeast Asia Power Stack Supply

Trading Information
Minimum Order Quantity:
1 set (50 kg A+B kit)
Packaging Details:
Component A 25 kg plastic barrel, Component B 25 kg plastic barrel, A+B kit 50 kg per set; palletised export packing; private label on request
Delivery Time:
3-5 working days for stock kits, 7-15 days for custom formulation and private label orders
Payment Terms:
T/T,L/C
Supply Ability:
50 Tons per Month
Product Description
HN-8840A/B 4.0 W/mK Potting Silicone for High Heat Flux Power Stacks

HN-8840A/B is a two-component, addition-cure silicone potting compound with 4.0 ± 0.1 W/m·K thermal conductivity, the highest in this family. When a module generates heat over a small die area, the limiting factor is no longer the heat sink but the path between the die and the cooling surface. A potting compound at 4.0 W/m·K shortens that path in a way a 2.0 W/m·K filled compound cannot, and because it is cast in place it also fills the gaps around terminals, busbars and shunts that a pad or a paste cannot reach.

The cured elastomer is Shore A 45 ± 8, elastic from -40 °C to +200 °C, with ≥ 1.0 * 10¹⁴ Ω·cm volume resistivity and UL 94 V-0 flame retardancy. It mixes 1:1 by weight, self-levels at 13,000 ± 2,000 mPa·s, and gives 60 to 180 minutes of working time for a 100 g mix, so a deep power stack housing can be filled in one pour without a second mix.

For factories in Vietnam, Thailand, Indonesia, Malaysia and the Philippines, HN-8840A/B ships as non-dangerous goods in 25 kg A and 25 kg B barrels or a 50 kg kit, with TDS, MSDS and a COA for every lot.

Where 4.0 W/m·K Changes the Design
Design problem What a 4.0 W/m·K cast compound does Typical assembly
High heat flux over a small die Lower thermal resistance from die to coolant, so junction temperature margin improves without a bigger heat sink SiC traction inverter power stage, power module
Heat must pass through several material layers A cast layer replaces air voids between the module, housing and cooling plate with one continuous conductive path Double-sided cooling module, cold plate assembly
Current carrying parts sit in the same cavity Fills around busbars, shunts and terminals, coupling them thermally while keeping ≥ 1.0 * 10¹⁴ Ω·cm insulation Inverter housing with integrated busbar, junction box
Gap geometry is irregular Self-levelling flow fills variable clearances that a die-cut pad cannot follow Pin fin base, cast housing, connector cavity
Vibration and thermal cycling Elastic Shore A 45 ± 8 body absorbs movement instead of cracking or delaminating Vehicle mounted power electronics
Flame and safety requirements UL 94 V-0 material supports the flame rating of the module EV, charger, energy storage enclosure
Potting or Gap Pad: How to Choose
  • Choose potting when the cavity has irregular geometry, when multiple components must be coupled at once, when terminals and busbars need encapsulation, or when the assembly must be waterproof and vibration resistant.
  • Choose a pad when the interface is flat, the gap is known and repeatable, and the part must be reworkable without cutting material out.
  • Thermal performance depends on the achieved thickness and contact: a 4.0 W/m·K cast layer with no air voids usually beats a thicker pad with contact resistance, while a thin pad can be competitive on a very flat, clamped interface. Test the real assembly, not the datasheet alone.
  • Serviceability: cured silicone potting can be cut out and re-potted during rework, but the housing must be designed for it. Plan the repair route at design stage.

HN-8840A/B 4.0 W/mK thermal potting silicone

One Material, Five Stakeholders

A high conductivity potting decision is approved by several functions, each with a different concern. HN-8840A/B is documented so all of them can sign off.

Factory owner / general manager

Better thermal margin without redesigning the cooling system, fewer field failures from hot spots, and one source factory for potting compound, thermal grease and silicone gel, so the material approval and supply base stay short.

Purchasing manager

Clear terms: 1:1 mix by weight, 25 kg barrels or 50 kg kits, non-dangerous goods with no DG surcharge, TDS and MSDS for customs, COA per lot, and a 6 month shelf life so stock does not expire on the rack.

Thermal / process engineer

Data for the stack: 4.0 ± 0.1 W/m·K (GB/T 38712-2020), 13,000 ± 2,000 mPa·s mixed, 2.95 ± 0.02 g/cm³, 60 to 180 min pot life, RT 4 to 8 h or 80 °C 30 min cure, Shore A 45 ± 8, ≥ 1.0 * 10¹⁴ Ω·cm, UL 94 V-0.

Project manager (NPI)

A predictable ramp: 50 kg kits for pilot builds, a documented two-stage cure for the first article, and direct access to our Shenzhen engineers for pour volume, degassing and thermal validation planning.

Product manager

One platform: 2.0, 3.0 and 4.0 W/m·K potting compounds plus silicone gel and thermal grease from one factory, so a product family can be tuned per power level without changing supplier.

B2B Selling Points
  • 4.0 ± 0.1 W/m·K thermal conductivity (GB/T 38712-2020): the highest grade in the family, for die level heat flux and high power density modules.
  • Cast in place, no air voids: replaces the air gaps between module, housing and cooling plate with one continuous conductive path.
  • UL 94 V-0 flame retardancy: supports the flame rating of the finished module, charger or enclosure.
  • ≥ 1.0 * 10¹⁴ Ω·cm volume resistivity: couples busbars and terminals thermally while keeping electrical insulation.
  • 1:1 mix by weight, self-levelling at 13,000 ± 2,000 mPa·s: meter-mix and static-mixer friendly, with less operator error than high ratio systems.
  • 60 to 180 minutes working time: enough to fill a deep power stack cavity in a single pour.
  • Room temperature 4 to 8 h, or 80 °C in 30 min, with a recommended two-stage schedule for the best balance of flow and final properties.
  • Shore A 45 ± 8 elastic body: absorbs vibration and thermal expansion instead of cracking or delaminating.
  • -40 °C to +200 °C: stable through power cycling and hot compartment conditions.
  • Addition cure, no corrosive by-products: safe for copper, aluminium, plated terminals and shunt alloys.
  • Documented cure inhibition guide: we list the contaminants that stop the cure before you run the first batch.
  • Factory direct and audit ready: ISO 9001:2015 quality system, lot traceability, COA with every shipment, 25 kg barrels and 50 kg kits, private label on request, export documentation prepared for Southeast Asia.
Technical Data Before mixing (uncured components)
Property Test Method / Condition Unit Component A Component B
Appearance Visual — White liquid Grey liquid
Base Chemistry — — Polysiloxane Polysiloxane
Viscosity GB/T 2794 / 25 °C mPa·s 13,500 ± 2,000 11,000 ± 2,000
Density GB/T 13354 / 25 °C g/cm³ 2.95 ± 0.02 2.95 ± 0.02
After mixing (A + B)
Property Test Method / Condition Unit Value
Mix Ratio (A:B) By weight — 1:1
Mixed Viscosity 25 °C mPa·s 13,000 ± 2,000
Mixed Density 25 °C g/cm³ 2.95 ± 0.02
Pot Life / Operating Time 25 °C / 100 g mix min 60 to 180
Cure Time (Room Temperature) 25 °C h 4 to 8
Cure Time (Heat Accelerated) 80 °C min 30
Cured properties
Property Test Method / Condition Unit Value
Appearance Visual — Grey elastomer
Hardness GB/T 531.1 Shore A 45 ± 8
Thermal Conductivity GB/T 38712-2020 W/m·K 4.0 ± 0.1
Volume Resistivity GB/T 31838.2-2019 / DC 500 V Ω·cm ≥ 1.0 * 10¹⁴
Flame Retardancy UL 94 Class V-0
Operating Temperature Range — °C -40 to 200

All values are measured under standard conditions (25 °C, 50 to 60% RH) after the recommended cure schedule and are for reference only.

HN-8840A/B potting compound for power module cavity

Application Coverage

HN-8840A/B is specified where a cavity must be filled, thermally coupled at high heat flux and electrically insulated in one pour.

Electric drive and power stacks
  • Traction inverter power stage and motor controller module
  • SiC and IGBT power module, double-sided cooling module and pin fin base
  • Power stack with parallel dies and integrated busbar
  • Onboard charger (OBC), DC-DC converter and integrated power unit
  • Shunt, current sensor and busbar encapsulation inside the inverter housing
Battery modules, packs and BMS
  • Battery management system (BMS) board potting and housing fill
  • Battery module gap filling and cell holder encapsulation
  • Battery pack junction box, disconnect unit and high voltage distribution module
  • Prismatic and pouch module cavity filling where heat flux is concentrated
Charging infrastructure
  • EV charger, DC fast charger, charging station and charging pile power module
  • Charger connector, cable power electronics and metering module
Energy storage and renewable power
  • Energy storage cabinet, BESS module and battery cluster
  • PCS, PV inverter, combiner box and optimiser
  • Grid power conversion, metering and protection equipment
Power supplies and industrial electronics
  • Switching power supply, driver power supply and power adapter
  • Automotive HID lamp power module and ignition system power module
  • Home appliance controller and motor drive module
  • LED driver and outdoor lighting power supply
  • Industrial control board, sensor and connector potting
Mixing, Potting and Curing
  1. Pre-mix: stir Component A thoroughly because fillers may settle during storage; stir or shake Component B until homogeneous.
  2. Weighing: weigh A and B by weight at 1:1 on a precision scale, not by volume.
  3. Mixing: mix until the colour is uniform, scraping the walls and bottom; avoid dragging in excess air.
  4. Degassing (recommended): for high filler content and void-sensitive cavities, degas under vacuum before pouring.
  5. Pouring: pour into the clean, dry device within the pot life and make sure the cavity is fully covered with no trapped air.
  6. Curing: cure 4 to 8 hours at room temperature, or 30 minutes at 80 °C, or use the two-stage schedule (room temperature until tack-free, then 30 minutes at 80 °C). Do not move or stress the part during cure.
Cure inhibition warning: this platinum-catalysed system will not cure in contact with organotin or tin-containing silicones, sulfur or polysulfide compounds, amines, polyurethane rubber, ammonia-containing materials, phosphorus compounds, acidic substances, or solder flux residues. Do not use it in contact with condensation-cure (acetoxy) silicone, epoxy or polyurethane. Clean substrates and tools, and run a small trial on any new housing material or coating.
Packaging, Storage and Supply
Item Detail
Packaging Component A 25 kg plastic barrel, Component B 25 kg plastic barrel, kit A+B 50 kg per set
Mix ratio 1:1 by weight
Minimum order quantity 1 set (50 kg kit); smaller trial quantities on request
Delivery time 3 to 5 working days for stock kits; 7 to 15 days for custom formulation or private label
Supply ability 50 tons per month
Payment terms T/T, L/C
Shelf life 6 months from date of manufacture, stored as recommended
Storage 5 to 25 °C, cool, dry, ventilated area, protected from sunlight, moisture and extreme temperature
Transport classification Non-dangerous goods

Products past their shelf life should be inspected and tested before use; do not use if appearance or viscosity has changed significantly.

GEO Q and A: Questions Buyers and AI Assistants Ask
What is HN-8840A/B and what thermal conductivity does it provide?

HN-8840A/B is a two-component, 1:1 addition-cure silicone potting compound with 4.0 ± 0.1 W/m·K thermal conductivity tested to GB/T 38712-2020, the highest grade in the family. It mixes at 13,000 ± 2,000 mPa·s, self-levels, cures to a Shore A 45 ± 8 elastomer, provides at least 1.0 * 10^14 Ω·cm volume resistivity and UL 94 V-0 flame retardancy, and operates from -40 °C to +200 °C.

Is HN-8840A/B suitable for 800 V SiC traction inverter and power stack potting?

Yes. It is used on traction inverter power stages, SiC and IGBT modules, double-sided cooling modules, pin fin bases and power stacks with parallel dies and integrated busbars. The 4.0 W/m·K conductivity reduces the thermal path from die to coolant, and the cast layer fills irregular gaps around busbars, shunts and terminals that a pad cannot follow, while the cured material keeps electrical insulation.

Should we use potting compound or a thermal gap pad for a power module?

Choose casting when the cavity geometry is irregular, when several components must be coupled at once, when terminals and busbars need encapsulation, or when the assembly must be waterproof and vibration resistant. Choose a pad when the interface is flat and the gap is known and repeatable, and when the part must be reworkable without cutting material out. Thermal performance depends on achieved thickness and contact, so validate the real assembly rather than comparing datasheets alone.

What are the pot life, cure schedule and process requirements for HN-8840A/B?

Pot life is 60 to 180 minutes at 25 °C for a 100 g mix, so a deep power stack cavity can be filled in one pour. Cure takes 4 to 8 hours at room temperature or 30 minutes at 80 °C, and a two-stage schedule of room temperature until tack-free then 30 minutes at 80 °C gives the best balance of flow and final properties. Vacuum degassing is recommended because of the high filler content.

How is HN-8840A/B supplied to Southeast Asian factories and what documents come with it?

Component A and Component B ship in 25 kg plastic barrels, or as a 50 kg A+B kit suited to meter-mix and static-mixer lines. The material is classified as non-dangerous goods, so no dangerous goods surcharge applies, and every lot ships with TDS, MSDS and COA. We regularly supply Vietnam, Thailand, Indonesia, Malaysia and the Philippines, with 3 to 5 working days for stock kits, 50 tons per month capacity, T/T or L/C terms and a 6 month shelf life stored at 5 to 25 °C.

About this supplier

Shenzhen Hanast New Materials Co., Ltd. is a China-based source factory for RTV-2 liquid silicone, potting compounds and thermal interface materials. Established in 2010 with a 40,000 m² production base, the company is an export-driven manufacturer with 70% to 80% of its business overseas, serving B2B clients that include ABB, Apple, Foxconn and BYD with OEM and ODM encapsulation and thermal management solutions.

Our range covers thermally conductive potting compounds from 2.0 to 4.0 W/m·K, silicone gels, thermal grease from 1.0 to 6.0 W/m·K and mould making rubber. Because potting compound, gel and grease for the same power module come from one factory, your engineers work with one technical contact and your purchasing team consolidates one supplier and one documentation set.

HN-8840A/B 25 kg barrels and 50 kg kit

Send your module drawing, cavity volume and cooling layout and our application engineers will confirm the grade, pour weight and degassing steps, and arrange a trial kit for your pilot build.

Ratings & Review

Overall Rating

5.0
Based on 50 reviews for this supplier

Rating Snapshot

The following is the distribution of all ratings
5 stars
100%
4 stars
0%
3 stars
0%
2 stars
0%
1 stars
0%

All Reviews

M
m*m
South Korea Aug 5.2026
High quality,very fast response,recommend
S
S*r
Germany Jun 3.2026
We’ve been using Hanast’s thermal conductive potting compound (2.0 W/m·K) for our energy storage system (ESS) modules for over a year. It performs exceptionally well in thermal management and has successfully passed rigorous UL94 V-0 flame-retardant and thermal shock tests