HN400 is a single-component, non-curing ultra-high thermal conductive silicone grease built on low thermal resistance fillers, with a thermal conductivity of 4.05 ± 0.1 W/m·K (ASTM D5470). It is supplied as a grey, glossy, fine paste with a worked penetration of 240 ± 20 (1/10 mm) and a specific gravity of 2.61 ± 0.08 g/cm³, which is exactly the consistency band that time-pressure dispensers, progressive cavity pumps, jet valves, screen printers and stencil printers handle without process re-tuning.
This grade is positioned for factories that have already decided to move from thermal pads, thermal tape and gap pads to a dispensable thermal interface material, or that are setting up a new charger, SiC module or heat sink assembly line and want one paste that behaves the same on the first article, on the pilot run and in mass production. Because the material never cures, there is no fixture time, no oven, no secondary cure step and no pot life countdown after the drum is opened.
| Line problem engineers raise | How HN400 answers it |
|---|---|
| Nozzle clogging and line stoppages between shifts | Single-component paste with no catalyst and no curing reaction, so nothing sets inside the nozzle or the static mixer. Material left in the reservoir stays paste until it is used. |
| Filler settling and hard packing in the drum | Oil separation ≤ 0.3 % and volatile matter ≤ 0.7 % (200 °C / 24 h), measured to SH/T 0324 and SH/T 0337. No hard settling that blocks the drum follower plate or pump inlet. |
| Dot height variation, stringing and satellites | Penetration 240 ± 20 (1/10 mm) gives a short, non-stringing paste body that releases cleanly from the needle at high cycle rates. |
| Pot life countdown and mixed-material waste | No A and B components, no pot life window, no purge-and-mix scrap. Left-over paste returns to the drum; open drums can be resealed and re-used. |
| Bond line thickness (BLT) too thick, thermal resistance too high | The paste spreads to a thin film under normal clamping, so BLT is set by hardware flatness and pressure, not by pad thickness tolerance. This is where a 4.0 W/mK grease beats a 3.0 W/mK pad of 0.5 mm or thicker. |
| Rework and re-seating after test failures | Non-curing paste can be wiped off with a lint-free cloth and re-applied, so a failed module can be reworked instead of scrapped. |
Most Southeast Asia charger and power module factories now run a mixed bill of materials. Use this table when the design team asks whether the pad can be swapped for a paste, or when purchasing asks why two interface materials are being stocked.
| Interface option | Typical BLT | Heat path | Rework | Best fit |
|---|---|---|---|---|
| Thermal pad / gap pad (pre-cut) | 0.5 – 3.0 mm, set by pad thickness | Through-pad conduction, thickness adds resistance | Pad is destroyed on removal | Large uneven gaps, no dispensing equipment, low volume builds |
| Thermal tape (adhesive backed) | 0.15 – 0.3 mm | Fixed by adhesive carrier, not serviceable | Not reworkable | Permanent small heat sinks, no clamping hardware |
| Phase change material | 0.05 – 0.2 mm after reflow | Very low at operating temperature only | Limited | Sealed modules, narrow operating window |
| HN400 4.0 W/mK non-curing grease | 0.05 – 0.15 mm typical in production | Metal-to-metal proximity with filler bridges at the interface | Wipe and re-apply | Clamped heat sink interfaces, SiC and IGBT modules, charger power stages, high volume lines with dispensing |
| Property | Test method / condition | Unit | Value |
|---|---|---|---|
| Appearance | Visual inspection | – | Grey, glossy, fine paste |
| Thermal conductivity | ASTM D5470 | W/m·K | 4.05 ± 0.1 |
| Specific gravity | GB/T 13354-1992 / 25 °C | g/cm³ | 2.61 ± 0.08 |
| Oil separation (oil bleed) | SH/T 0324-1992 / 200 °C, 24 h | % | ≤ 0.3 |
| Volatile matter | SH/T 0337-92 / 200 °C, 24 h | % | ≤ 0.7 |
| Penetration (cone penetration) | GB/T 269-2023 / 25 °C | 1/10 mm | 240 ± 20 |
| Breakdown voltage | IEC 60243 / 0.20 mm thickness | V/mm | 1100 |
| Operating temperature range | – | °C | −50 to +200 |
| Compliance | RoHS 2.0 | – | Compliant |
Values are measured under standard conditions and are for reference only. Actual thermal performance depends on bond line thickness, surface flatness and contact pressure, so confirm the interface design on your own heat sink and module before releasing the drawing.
Where HN400 is used: 24 application points across the new energy vehicle and power electronics chain EV charging and onboard power![]()
For the factory owner and plant manager
One paste covers the charger line, the module line and the heat sink line, so tooling, training and incoming inspection stay single-source. Non-curing means no oven, no cure fixtures and no energy cost per module. A wipe-and-reapply rework route protects the value of a finished module instead of scrapping it at final test. Bulk 5 kg drums replace small syringes, which cuts packaging waste and operator handling time on high-volume shifts.
For the purchasing and procurement team
Minimum order quantity is 1 kg, 5 kg plastic drums are the standard supply pack, and custom pack sizes are available on request. Supply capacity is 50 tons per month, which covers a ramp-up from pilot run to mass production without a second source. Each shipment leaves with a technical data sheet and a safety data sheet, and batch level certificates of analysis can be issued on request so incoming quality control has a document trail. Transport is classified as non-dangerous goods, so sea freight and air freight bookings do not need a dangerous goods declaration.
For the process and manufacturing engineer
HN400 can be applied by brushing, rolling, automatic dispensing, screen printing and stencil printing. Because viscosity stays constant through the shift, dot volume does not drift with time as it does with a curing two-component gel. Recommended line practice: clean and dry the interface first, dispense a cross or dot pattern that covers 60 to 80 percent of the contact area, assemble immediately, then torque the fasteners to the heat sink supplier spec so the paste squeezes to the thinnest stable film. Wipe excess at the edges with a lint-free cloth before cure-free assembly is closed.
For the reliability and quality engineer
Low oil separation and low volatility are the two numbers that decide whether a grease dries out, pumps out or fogs an optical surface over service life. HN400 is specified at 0.3 percent oil separation and 0.7 percent volatility after 24 hours at 200 °C, and it keeps paste consistency from minus 50 to plus 200 °C without hardening or cracking. It resists water, ozone and weathering, and has near-zero free radical content. Ask us for the current batch data and run your own thermal cycling and high temperature storage test before design freeze.
For the project and product manager
The HN family is a graded platform, so a product line can be positioned without changing supplier: 1.0 W/mK insulating grade for transformer and power supply interfaces, 2.0 W/mK general grade, 2.95 W/mK clamped module grade, 4.0 W/mK HN400 for charger and SiC module interfaces, and metal-filled 5.0 to 6.0 W/mK grades for CPU and GPU cooling. Sampling is a 1 kg drum, and the sample, pilot run and mass production steps use the same formulation, so a design validation done on the sample stays valid after ramp up.
| Step | Action |
|---|---|
| 1. Surface preparation | Clean both contact surfaces with a solvent to remove grease, dust and oxidation, then let them dry completely. |
| 2. Application | Apply by brush, roller, automatic dispenser or screen printing. Keep the deposit pattern inside the heat sink footprint. |
| 3. Spreading | Spread evenly with a clean blade, plastic spatula or dispensing pass to the target thickness. Thinner is better for heat transfer. |
| 4. Thickness control | Excess paste does not improve conduction and can reduce it. Remove overflow at the edges with a lint-free cloth. |
| 5. Assembly | Assemble the heat sink immediately and torque fasteners to specification to set a stable bond line thickness. |
Yes. HN400 is a single-component non-curing paste, so there is no mixed material that can gel inside the needle, valve or static mixer, and nothing sets in the reservoir during a shift. It is specified at 240 ± 20 penetration and 2.61 g/cm³ specific gravity, close to a standard filled silicone grease, so start from the pump, needle and pressure settings you already use for a filled thermal paste of the same density, then adjust dot volume to your BLT target. Because oil separation is 0.3 percent or lower, filler does not hard-pack in the drum and block the follower plate.
Is a 4.0 W/mK grease really better than the thermal pad we use today?In a clamped, flat interface, usually yes. A pad conducts through its full thickness, so a 1.0 mm pad adds resistance that the paste does not, because the paste is squeezed down to a 0.05 to 0.15 mm film and the heat path runs almost metal to metal with filler bridges. Paste also wets the surface and fills micro scratches. A pad still wins on very uneven gaps, on designs without clamping hardware, and on lines with no dispensing equipment. The practical answer is to keep pads where the gap is mechanical, and specify HN400 where the gap is flat and the interface is clamped.
Which specifications should appear on our incoming inspection sheet?Ask the supplier for thermal conductivity by ASTM D5470, specific gravity, oil separation and volatile matter at 200 °C for 24 hours, penetration at 25 °C, and breakdown voltage at 0.20 mm. For HN400 that is 4.05 ± 0.1 W/m·K, 2.61 ± 0.08 g/cm³, oil separation 0.3 percent maximum, volatile matter 0.7 percent maximum, penetration 240 ± 20, breakdown voltage 1100 V/mm, operating range minus 50 to plus 200 °C, RoHS 2.0 compliant. These are the numbers that predict line behaviour and long term stability, not a single headline conductivity figure.
How do we qualify HN400 without stopping the charger line?Three steps. First, request a 1 kg sample drum and run a first article on one heat sink and module pair, then measure case temperature against your current interface at the same load. Second, run a short pilot lot on the real dispensing equipment to confirm dot repeatability, cycle time and rework handling. Third, freeze the process with a drawing that states BLT target, deposit pattern and torque spec, and request the batch certificate of analysis with each delivery so incoming quality control can compare against the sample. The formulation does not change between sample, pilot and mass production.
What are the lead time, packaging and documentation for a Southeast Asia order?MOQ is 1 kg. Standard packs are 1 kg and 5 kg plastic drums with custom pack sizes on request. Supply capacity is 50 tons per month and lead time is typically 7 to 15 days depending on pack size and customisation. Each order ships with a technical data sheet and a safety data sheet, batch certificates of analysis are available on request, and the product is classified as non-dangerous goods for sea and air freight to Vietnam, Thailand, Indonesia, Malaysia and the Philippines. Share your module drawing or heat sink specification and our application engineers will confirm the grade, the deposit pattern and the BLT target before you release the purchase order.
About this supplierShenzhen Hanast New Materials Co., Ltd. is a China-based source factory for RTV-2 liquid silicone, potting compounds and thermal interface materials. Established in 2010 with a 40,000 m² production base, the company is an export-driven manufacturer with 70 to 80 percent of its business overseas, supplying B2B clients with OEM and ODM encapsulation and thermal management solutions.
Our product range covers thermal grease from 1.0 to 6.0 W/m·K, thermally conductive potting compounds, silicone gels, mould making rubber and food grade silicone. Because the thermal grease and the potting compound for the same module come from one factory, your engineering team works with one technical contact and your purchasing team consolidates one supplier, one documentation set and one shipment schedule.
![]()
Send your module drawing or heat sink specification and our application engineers will recommend the grade and bond line thickness, and arrange a 1 kg sample drum for your trial build.
Tell us your charging power level, the interface area and your current pad thickness, and we will reply with the matching HN400 deposit pattern and a delivery schedule for Southeast Asia.