HN100 is a single-component, non-curing insulating silicone thermal grease rated 1.0 ± 0.1 W/m·K (ASTM D5470) with dielectric strength of 2450 V/mm at 0.20 mm (IEC 60243), specific gravity 1.85 ± 0.08 g/cm³ and penetration 370 ± 20 (1/10 mm). It holds paste consistency from −50 °C to +200 °C, shows no powdering after 8 days of continuous 200 °C baking and no drying after 3 hours on a 280 °C heating platform, and is RoHS 2.0 compliant, non-toxic, odourless and non-corrosive.
This page is written for the people who have to approve a material rather than develop one: the EMS plant buyer, the brand owner outsourcing assembly, the sourcing manager adding a second source, and the quality team that has to close an audit finding. The technical data below is the same grade as our standard HN100; what this presentation adds is the documentation package, traceability, change control and landed cost model that a factory audit actually asks for.
![]()
Audit findings on thermal interface materials are almost never about conductivity. They are about paper: a missing SDS, a certificate of analysis without a batch number, or a supplier that cannot say which drum went into which shipment. Below is what we issue, and what a buyer should request from any grease supplier.
| Document | What it answers in an audit | When it is issued |
|---|---|---|
| Technical data sheet (TDS) | Specification, test methods, operating limits, packaging and storage instructions | With quotation and with every shipment |
| Safety data sheet (SDS) | Hazard classification, handling, first aid, transport status | With every shipment, and on request at quotation stage |
| Batch certificate of analysis (COA) | Measured values for conductivity, gravity, penetration, oil separation, volatility, breakdown voltage against the TDS limits | Per batch, on request or attached to the shipping documents |
| RoHS 2.0 declaration | Restricted substance compliance for the finished paste | With quotation, refreshed on request |
| Batch and lot traceability record | Which production batch filled which drum, which drum went into which carton and shipment | Maintained per lot, provided on request for audit or complaint investigation |
| Change notification (PCN) | Notice before any formulation, raw material source, packaging or plant change that affects the approved part | Issued before the change takes effect on your part number |
| Transport classification statement | Confirms non-dangerous goods status so freight forwarders do not require DG handling | With shipping documents |
Most Southeast Asia assembly plants are now asked by their customers to name a second source for every critical material. With a non-curing paste, dual sourcing is simpler than with a two-component system, because there is no mix ratio, no pot life and no cure schedule to re-qualify.
| Step | What happens | Audit evidence you keep |
|---|---|---|
| 1. Sample | 1 kg drum from the production batch, with COA of that batch | Sample COA filed against the approved part number |
| 2. Pilot run | Same formulation run on your dispenser or screen printer, film thickness and coverage recorded | Process parameter sheet and first article inspection report |
| 3. Approval | Drawing frozen with film thickness target, deposit pattern and torque spec | Approved supplier list entry with the grade, pack size and TDS revision |
| 4. Mass production | Same formulation, same plant, same test methods, COA per batch | Incoming inspection record comparing each lot to the approved sample |
Because the grade does not cure, there is nothing in the material that changes state during storage or use, so the validation performed on the sample stays representative of production. That is the argument to put in front of your customer when they ask why the second source needs no new reliability programme: the material is thermodynamically the same paste at shipment and at assembly.
Incoming inspection: what to measure and how often| Check | Method | HN100 limit | Frequency |
|---|---|---|---|
| Thermal conductivity | ASTM D5470 | 1.0 ± 0.1 W/m·K | Per batch COA, verify annually in house |
| Breakdown voltage | IEC 60243 at 0.20 mm | 2450 V/mm | Per batch COA, verify on new supplier or new plant |
| Specific gravity | GB/T 13354-1992 at 25 °C | 1.85 ± 0.08 g/cm³ | Every incoming lot, fast and cheap |
| Penetration | GB/T 269-2023 at 25 °C | 370 ± 20 (1/10 mm) | Every incoming lot, catches consistency drift |
| Oil separation | SH/T 0324-1992, 200 °C, 24 h | ≤ 0.3 % | Per batch COA, verify in house on new batches |
| Volatile matter | SH/T 0337-92, 200 °C, 24 h | ≤ 0.6 % | Per batch COA, verify in house on new batches |
| Appearance and packaging | Visual | White or grey paste, sealed drum, label matches COA batch | Every incoming lot |
Specific gravity and penetration are the two checks we recommend on every incoming lot: they are quick, they need little equipment, and they catch the filling mistakes and raw material substitutions that a certificate alone will not reveal.
Landed cost model for a heat sink interfacePurchasing decisions on thermal interface materials are usually decided on price per kilogram, which is the wrong unit. The comparable unit is cost per assembled module, and it has six components.
| Cost element | What drives it | How HN100 behaves |
|---|---|---|
| Material per module | Contact area × film thickness × density | 1.85 g/cm³ and thin film application keep grams per module low; a 25 cm² interface at 0.1 mm uses about 0.46 g |
| Packaging | Container type and disposal | 1 kg and 5 kg plastic drums, custom pack sizes; 5 kg drums reduce handling on high volume lines |
| Freight | Weight, dangerous goods status | Classified as non-dangerous goods, so no DG surcharge and no DG documentation on sea or air freight |
| Duty and origin | HS code and certificate of origin | Shipped from Shenzhen with the commercial invoice and origin documents the destination customs broker requests |
| Process cost | Dispensing, cure, rework | No curing step, no oven, no fixture; rework is wipe and re-apply instead of scrap |
| Scrap and yield | Interface related failures | Non-curing paste can be re-seated, so end of line failures are recoverable |
Model it as material plus packaging plus freight plus process labour plus yield loss, divided by good modules shipped. On most lines the process and scrap terms dominate, and that is where a non-curing paste removes cost that a pad or a heat cure system adds back.
OEM packaging, labelling and shipment for importers| Property | Test method / condition | Unit | Value |
|---|---|---|---|
| Appearance | Visual inspection | – | White or grey paste |
| Thermal conductivity | ASTM D5470 | W/m·K | 1.0 ± 0.1 |
| Specific gravity | GB/T 13354-1992 / 25 °C | g/cm³ | 1.85 ± 0.08 |
| Oil separation (oil bleed) | SH/T 0324-1992 / 200 °C, 24 h | % | ≤ 0.3 |
| Volatile matter | SH/T 0337-92 / 200 °C, 24 h | % | ≤ 0.6 |
| Penetration (cone penetration) | GB/T 269-2023 / 25 °C | 1/10 mm | 370 ± 20 |
| High temperature stability | 200 °C constant temperature oven, 0.2 mm film | – | No powdering after 8 days continuous baking |
| Temperature resistance | Heating platform 280 °C, 0.2 mm film | – | No drying after 3 hours continuous baking |
| Breakdown voltage | IEC 60243 / 0.20 mm thickness | V/mm | 2450 |
| Operating temperature range | – | °C | −50 to +200 |
| Compliance | RoHS 2.0, non-toxic, odourless, non-corrosive | – | Compliant |
Values are measured under standard conditions and are for reference only. Actual thermal performance depends on film thickness, surface flatness and contact pressure, so confirm the interface on your own hardware and keep the approved TDS revision in your supplier file.
Applications: 26 interface points across new energy vehicle, power supply and appliance assembly New energy vehicle and charging hardwareFor the factory owner and plant manager
One grade covers the charger line, the power supply line and the service bench, so inventory is a single part number in 1 kg and 5 kg drums instead of several pad thicknesses. No cure step means no oven, no fixtures and no queue time before the next station, and a failed unit can be wiped and re-applied instead of scrapped.
For the purchasing and procurement team
MOQ is 1 kg, capacity is 50 tons per month and lead time is typically 7 to 15 days. Each shipment carries TDS, SDS and packing details, batch COAs are available on request, change notification is issued before any formulation or plant change, and non-dangerous goods classification keeps freight simple. Compare suppliers on cost per good module and on document completeness, not on price per kilogram alone.
For the process and manufacturing engineer
Apply by brush, roller, automatic dispensing or screen printing after solvent cleaning and drying. Freeze film thickness target, deposit pattern and torque spec in the assembly drawing, and record the dispenser parameters in the process sheet so a second line or a second shift reproduces the same interface. Penetration 370 ± 20 keeps the paste workable at thin film without stringing.
For the quality and reliability engineer
Use specific gravity and penetration on every incoming lot, and the full COA set on each batch. The two stability results that predict field behaviour are no powdering after 8 days at 200 °C and no drying after 3 hours at 280 °C on a 0.2 mm film; oil separation up to 0.3 percent and volatile matter up to 0.6 percent predict whether an interface dries out or fogs over time. Keep the approved sample sealed and labelled with its COA for comparison.
For the project and product manager
The HN family is a graded platform that can be positioned without changing supplier: 1.0 W/mK HN100 for insulating power supply interfaces, 2.05 W/mK HN200 for general electronics, 2.95 W/mK HN300 for clamped modules, 4.05 W/mK HN400 for charger and SiC interfaces, and metal-filled 5.0 to 6.0 W/mK grades for CPU and GPU duty. One supplier, one document set and one technical contact reduces the qualification workload when a product line expands.
| Grade | Conductivity | Dielectric strength | Temperature range | Best fit |
|---|---|---|---|---|
| HN100 | 1.0 W/m·K | 2450 V/mm | −50 to +200 °C | Insulating power supply, transformer, PTC heater, thermostat |
| HN200 | 2.05 W/m·K | 2450 V/mm | −50 to +200 °C | LED driver, adapter, general heat sink mounting |
| HN300 | 2.95 W/m·K | 1850 V/mm | −40 to +180 °C | Clamped power module, cold plate interface |
| HN400 | 4.05 W/m·K | 1100 V/mm | −50 to +200 °C | EV charger and SiC module, high heat flux |
| HN500 and HN600 | 5.0 to 6.0 W/m·K | Metal-filled duty | – | CPU, GPU and server cooling |
| Step | Action |
|---|---|
| 1. Surface preparation | Clean both surfaces with a solvent to remove grease, dust and oxidation, then dry completely. |
| 2. Application | Apply by brush, roller, automatic dispenser or screen printing, keeping the deposit inside the contact land area. |
| 3. Spreading | Spread evenly to the target film thickness. A thinner film transfers heat better than a thick one. |
| 4. Thickness control | Remove excess at the edges with a lint-free cloth to avoid paste entering creepage paths. |
| 5. Assembly | Assemble immediately and torque fasteners to specification to set a stable film thickness. |
Every shipment carries a technical data sheet, a safety data sheet and the packing information, and batch certificates of analysis are issued on request against the batch number printed on the drum. Batch and lot traceability records link the production batch to the drum and to the shipment, and change notification is issued before any formulation, raw material source, packaging or plant change that affects your approved part. That set is what an EMS audit typically asks for on a thermal interface material.
Can we add HN100 as a second source without running a new reliability programme?In most cases yes, and the reason is that the material is non-curing: there is no mix ratio, no pot life and no cure schedule, so nothing in the paste changes state between shipment and assembly. The qualification that matters is the interface, so run a 1 kg sample from a production batch through your dispenser, compare film thickness and coverage against your current material, and file the sample COA with the first article report. Your reliability test on the assembly then covers both sources if the film thickness target is the same.
Which incoming checks catch a bad batch fastest?Specific gravity and penetration. Both are quick, need little equipment and are sensitive to filling errors and raw material substitution, so they catch the majority of lot to lot problems before the material reaches the line. Add oil separation and volatile matter when a new batch is opened for a critical product, and compare every value against the approved sample rather than only against the pass or fail limit.
What are the MOQ, pack sizes, lead time and shipping terms to Southeast Asia?MOQ is 1 kg. Standard packs are 1 kg and 5 kg plastic drums with custom sizes on request, and private label labelling can be agreed at order stage. Capacity is 50 tons per month and lead time is typically 7 to 15 days. The product is classified as non-dangerous goods, so sea and air freight to Vietnam, Thailand, Indonesia, Malaysia and the Philippines requires no dangerous goods handling, and shelf life of 12 months below 27 °C allows consolidated sea shipments.
How do we compare the true cost of a pad against HN100 per module?Convert both to cost per good module. For the paste, multiply contact area by film thickness and density to get grams per module, then add packaging, freight, dispensing labour and scrap; for a 25 cm² interface at 0.1 mm that is about 0.46 g of paste at 1.85 g/cm³. For a pad, add the pad part number, die cutting, placement labour and the scrap caused by thickness tolerances. In most builds the labour and scrap terms decide the result, and a non-curing paste with rework capability removes cost that a pad or a heat cure system adds back.
About this supplierShenzhen Hanast New Materials Co., Ltd. is a China-based source factory for RTV-2 liquid silicone, potting compounds and thermal interface materials. Established in 2010 with a 40,000 m² production base, the company is an export-driven manufacturer with 70 to 80 percent of its business overseas, supplying B2B clients with OEM and ODM encapsulation and thermal management solutions.
Our range covers thermal grease from 1.0 to 6.0 W/m·K, thermally conductive potting compounds, silicone gels, mould making rubber and food grade silicone. Because the thermal grease and the potting compound for the same assembly come from one factory, your engineering team works with one technical contact and your purchasing team consolidates one supplier, one documentation set and one shipment schedule.
![]()
Send your approved part number, TDS revision and audit checklist and our team will return the matching grade, the document package for your supplier file and a 1 kg sample from a production batch for your pilot run.
Tell us the interface area, working voltage and annual volume, and we will reply with the cost per module estimate and a shipment schedule for Southeast Asia.