Home > Products >
Thermal Grease Paste
>
5.00 W/mK Metal-Filled Non-Curing Thermal Grease Paste for AI Server GPU IHS Cooling

5.00 W/mK Metal-Filled Non-Curing Thermal Grease Paste for AI Server GPU IHS Cooling

Product Details:
Place of Origin: Shenzhen, Guangdong, China
Brand Name: HANAST
Certification: RoHS 2.0, halogen-free, REACH
Model Number: HN500
Detail Information
Place of Origin:
Shenzhen, Guangdong, China
Brand Name:
HANAST
Certification:
RoHS 2.0, halogen-free, REACH
Model Number:
HN500
Thermal Conductivity:
5.05 ± 0.1 W/m·K
Specific Gravity:
2.6 ± 0.1 G/cm³
Penetration:
290 ± 20 (1/10 Mm)
Dielectric Strength:
1100 V/mm At 0.20 Mm
Operating Temperature:
−40 °C To +200 °C
Oil Separation:
≤ 0.3 % (200 °C, 24 H)
Highlight:

High Light

Highlight:

Liquid Metal Alternative Non-Conductive Paste

,

AI Server GPU IHS Grease

,

Southeast Asia Data Center Grease Supply

Trading Information
Minimum Order Quantity:
1 kg
Packaging Details:
1 kg and 5 kg plastic drums, custom pack sizes on request
Delivery Time:
7 to 15 days
Payment Terms:
T/T,L/C
Supply Ability:
50 tons per month
Product Description
HN500 5.00 W/mK metal-filled grease as a liquid metal alternative

HN500 is a single-component, non-curing, metal-filled silicone thermal grease rated 5.00 ± 0.1 W/m·K (ASTM D5470) with a low bond line thickness and a grey, glossy, fine paste texture at 2.6 ± 0.1 g/cm³ and 290 ± 20 penetration (1/10 mm). It is specified from −40 °C to +200 °C, with oil separation of 0.3 percent or less and volatile matter of 0.7 percent or less at 200 °C for 24 hours, and it complies with RoHS 2.0, halogen-free and REACH.

The grade exists for one specific decision that many hardware teams now face: the thermal budget says liquid metal, but the product needs to survive volume manufacturing, field service and a warranty without the risk that comes with a conductive fluid. HN500 gives most of the thermal gain of metal-filled chemistry in a non-liquid, non-curing paste that can be dispensed, screen printed, wiped and re-applied on a normal line.

HN500 metal-filled thermal grease on a GPU heat sink interface
Liquid metal versus metal-filled silicone grease
Decision factor Liquid metal (gallium alloy) HN500 metal-filled grease
Bulk thermal conductivity Very high, typically an order of magnitude above filled grease 5.05 ± 0.1 W/m·K, the highest grade in the HN range
Electrical behaviour Electrically conductive, a spill across the board is a short circuit risk Dielectric strength 1100 V/mm at 0.20 mm, so a thin film is not a conductive bridge in normal use
Aluminium contact Attacks and amalgamates aluminium, so nickel plating is required Silicone based, safe with aluminium, copper and nickel plated surfaces
Application Syringe, easy to over-apply, hard to control BLT Brush, roller, automatic dispensing or screen printing with a controlled deposit
Rework and service Difficult to remove fully, contaminates the socket Wipe with a lint-free cloth and re-apply, no alloy residue
Shipping and handling Restricted, and a spill procedure is required Classified as non-dangerous goods, standard industrial handling
Best fit Benchmarking, extreme overclocking, non-aluminium nickel plated cold plates Volume production, AI server and GPU modules, OBC and industrial drives where safety and serviceability matter
Application restriction: HN500 is metal-filled. Dielectric strength of 1100 V/mm at 0.20 mm is a thin film property, not an insulation rating. Do not apply it to exposed live parts, bare circuit boards or uninsulated conductors, and keep it out of any dimension a safety standard measures as creepage or clearance.
Why low BLT is the whole point at 5 W/mK

Interface resistance is bond line thickness divided by thermal conductivity. At 5.05 W/m·K the material term is small, so the film thickness becomes the dominant variable in the interface. The table below is the pure conduction term, calculated as BLT divided by 5.05 W/m·K, before contact resistance is added.

Bond line thickness Conduction term at 5.05 W/m·K Same film with a 3.0 W/m·K paste
0.02 mm 0.040 °C·cm²/W 0.067 °C·cm²/W
0.05 mm 0.099 °C·cm²/W 0.167 °C·cm²/W
0.10 mm 0.198 °C·cm²/W 0.333 °C·cm²/W

Two practical readings. First, going from a 3 W/mK paste to HN500 at the same 0.10 mm film roughly halves the conduction term, which is why an upgrade on a thermally limited server or GPU module is measurable. Second, doubling the film from 0.05 mm to 0.10 mm costs more than the entire conductivity upgrade gains, so the mounting pressure, surface flatness and deposit volume matter more than the datasheet headline. Control the film and the paste pays you back; ignore the film and no grade will save the design.

Mounting and process notes for IHS and heat sink interfaces
Interface type What controls the film What to specify
CPU or GPU integrated heat spreader to cooler base Mounting pressure and cooler flatness Even screw torque in a cross pattern, target pressure from the cooler vendor, single thin line or dot pattern rather than a full flood
AI accelerator module and cold plate Module frame pressure and cold plate flatness Pressure band on the drawing, flatness check on the cold plate, no gap at the module corners
Server 1U and rack mounted heat sink Spring loaded screws and standoff height Standoff height tolerance, spring specification, film target recorded in the assembly instruction
Vapour chamber and heat pipe base Base flatness and contact area Deposit pattern matched to the actual land area, not the full heat sink footprint
OBC and power module base plate Frame bolts and thermal pad replacement Film target and torque spec in the drawing, keep the paste out of the isolation path
Technical data (TDS HANAST-TDS-022 Rev.1)
Property Test method / condition Unit Value
Appearance Visual inspection – Grey, glossy, fine paste
Thermal conductivity ASTM D5470 W/m·K 5.05 ± 0.1
Specific gravity GB/T 13354-1992 / 25 °C g/cm³ 2.6 ± 0.1
Oil separation (oil bleed) SH/T 0324-1992 / 200 °C, 24 h % ≤ 0.3
Volatile matter SH/T 0337-92 / 200 °C, 24 h % ≤ 0.7
Penetration (cone penetration) GB/T 269-2023 / 25 °C 1/10 mm 290 ± 20
Breakdown voltage IEC 60243 / 0.20 mm thickness V/mm 1100
Operating temperature range – °C −40 to +200
Compliance RoHS 2.0, halogen-free, REACH – Compliant

Values are measured under standard conditions and are for reference only. Actual thermal performance depends on bond line thickness, surface flatness and contact pressure, so verify the interface on your own hardware and record the approved TDS revision in the supplier file.

Applications: 27 interface points across servers, automotive power and industrial control
Server, AI and data centre cooling
  • AI training and inference accelerator module to cold plate
  • GPU card and graphics card die to heat sink interface
  • Server CPU, 1U heat sink and rack mounted cooling module
  • High performance processor and chipset integrated heat spreader
  • Vapour chamber, heat pipe and heat sink assembly base
Automotive electronics and new energy vehicle
  • Onboard charger (OBC) power stage to housing
  • DC-DC converter and inverter control module interface
  • Automotive electronics and ADAS controller heat sink
  • Battery management board and power module base plate
  • LED headlamp driver and vehicle lighting module
Power conversion and industrial control
  • Photovoltaic inverter and combiner power stage
  • PLC, electrical control system and servo drive heat sink
  • Switching power supply, rectifier and regulator module
  • Welding inverter and induction heating power stack
  • UPS and telecom rectifier thermal interface
Network, computing and consumer hardware
  • Network communication equipment and base station module
  • Router, switch and optical module heat sink
  • Industrial PC, embedded computer and edge device
  • Notebook, gaming laptop and small form factor cooler
  • Microwave device and voltage regulator coating or encapsulation
Assembly and service points
  • Heat sink re-seating after service or upgrade
  • CPU, GPU and PLC replacement paste application

5.00 W/mK Metal-Filled Non-Curing Thermal Grease Paste for AI Server GPU IHS Cooling

What each stakeholder should check before approving HN500

For the factory owner and plant manager

HN500 removes the two costs that liquid metal brings into a factory: a controlled spill and contamination procedure, and a rework route that cannot clean the socket. Because it is a non-curing paste on a standard dispensing line, existing equipment and operators apply it without new tooling, and end of line failures can be wiped and re-applied instead of scrapped.

For the purchasing and procurement team

MOQ is 1 kg, standard packs are 1 kg and 5 kg plastic drums with custom sizes on request, capacity is 50 tons per month and lead time is typically 7 to 15 days. Every shipment carries TDS and SDS, batch COAs are available on request, and transport is classified as non-dangerous goods, unlike many liquid metal products, so sea and air freight to Vietnam, Thailand, Indonesia, Malaysia and the Philippines stays simple.

For the thermal and mechanical engineer

Treat film thickness as the primary design variable: at 5.05 W/mK, going from 0.05 mm to 0.10 mm adds more resistance than the upgrade from a 3 W/mK paste gained. Specify the mounting pressure band, check cooler and IHS flatness, and use a dot or line deposit pattern instead of flooding the interface. If the design currently calls for liquid metal, run an A/B test at your real power level before committing, since the paste loses some bulk conductivity but gains a stable, serviceable interface.

For the quality and reliability engineer

Put conductivity, specific gravity, penetration, oil separation and volatile matter on the incoming inspection sheet, and track pump-out on your own power cycling test, because that is the real long term risk on a high heat flux interface rather than conductivity drift. Low volatility of 0.7 percent or less at 200 °C matters for sealed enclosures where outgassing can fog optics or deposit on nearby surfaces.

For the project and product manager

The HN family lets one product line span from insulating to highest conductivity without changing supplier: 1.0 W/mK HN100, 2.05 W/mK HN200, 2.95 W/mK HN300, 4.05 W/mK HN400 and 5.05 W/mK HN500 for the top of the range. Sampling is a 1 kg drum and the formulation is identical from sample to mass production, so a design validation on the sample stays valid through ramp up.

Grade selection inside the HN thermal grease family
Grade Conductivity Filler Dielectric strength Temperature range Best fit
HN100 1.0 W/m·K Silicone 2450 V/mm −50 to +200 °C Insulating power supply, transformer, PTC heater
HN200 2.05 W/m·K Silicone 2450 V/mm −50 to +200 °C LED driver, adapter, general heat sink
HN300 2.95 W/m·K Silicone 1850 V/mm −40 to +180 °C Clamped power module, cold plate
HN400 4.05 W/m·K Silicone 1100 V/mm −50 to +200 °C EV charger and SiC module
HN500 5.05 W/m·K Metal-filled 1100 V/mm −40 to +200 °C AI server, GPU, OBC, PV inverter, PLC
Application instructions
Step Action
1. Surface preparation Clean both surfaces with a solvent to remove grease, dust and oxidation, then dry completely. Remove any old paste residue fully, especially after a liquid metal trial.
2. Application Apply by brush, roller, automatic dispenser or screen printing. Use a dot or thin line pattern so the film forms under mounting pressure.
3. Spreading Spread evenly to the target film thickness. A thin film transfers heat better than a thick one at this conductivity.
4. Thickness control Remove excess at the edges with a lint-free cloth. Excess paste does not improve conduction and can reduce it.
5. Assembly Assemble immediately and torque fasteners evenly in a cross pattern to set a stable bond line thickness.
Packaging, storage and handling
  • Standard packs 1 kg and 5 kg plastic drums. Custom pack sizes available on request.
  • Store sealed below 27 °C, cool, dry and ventilated, away from direct sunlight. Shelf life 12 months when unopened.
  • Stir thoroughly before use if a small amount of silicone oil separates during storage. Performance is not affected.
  • Industrial use only. Wear nitrile gloves and safety goggles, ventilate the work area and avoid skin and eye contact. For eye contact rinse with clean water for 10 to 15 minutes and seek medical attention.
Q and A for hardware, process and sourcing teams
Is HN500 a real replacement for liquid metal in an AI server or GPU module?

It is a replacement for the applications where liquid metal is chosen for thermal gain but its conductivity and aluminium incompatibility are a liability. HN500 gives 5.05 W/mK in a non-curing paste with 1100 V/mm dielectric strength at 0.20 mm and no alloying reaction with aluminium. Where the design needs the absolute maximum conductivity on a nickel plated cold plate and can control a conductive fluid, liquid metal is still the higher number. Where the product needs volume assembly, serviceability and a warranty, the paste is the practical choice, and an A/B test at your real power level will show whether the thermal difference is inside your margin.

How much does bond line thickness actually change the result at 5 W/mK?

A lot. The conduction term is BLT divided by conductivity, so at 5.05 W/mK a 0.05 mm film is about 0.099 °C·cm²/W and a 0.10 mm film is about 0.198 °C·cm²/W. Doubling the film doubles the resistance, which costs more than the entire upgrade from a 3 W/mK paste to a 5 W/mK paste at the same thickness. That is why mounting pressure, flatness and deposit volume deserve more attention than the conductivity figure.

Can HN500 be used on aluminium heat sinks without plating?

Yes. HN500 is a silicone based metal-filled paste, not a gallium alloy, so it does not amalgamate aluminium the way liquid metal does. Standard aluminium, copper and nickel plated surfaces are all acceptable. Clean the surface properly and remove any previous liquid metal residue completely before applying, because residual alloy on the surface is the contamination risk, not the paste itself.

What are the MOQ, packaging, lead time and shipping classification for Southeast Asia?

MOQ is 1 kg, standard packs are 1 kg and 5 kg plastic drums with custom sizes on request, capacity is 50 tons per month and lead time is typically 7 to 15 days. Each shipment includes TDS and SDS, batch COAs are available on request, and the product is classified as non-dangerous goods, so sea and air freight to Vietnam, Thailand, Indonesia, Malaysia and the Philippines requires no dangerous goods handling.

Which parameters should we monitor for long term stability on a high power interface?

Monitor pump-out and dry-out rather than conductivity. The indicative numbers are oil separation of 0.3 percent or less and volatile matter of 0.7 percent or less at 200 °C for 24 hours, both of which limit how much the paste can lose over service life, and the non-curing nature means there is no hardening or cracking from a cure reaction. Run a power cycling test on your own module and inspect the interface after cycling for dry patches or edge migration before you freeze the design.

About this supplier

Shenzhen Hanast New Materials Co., Ltd. is a China-based source factory for RTV-2 liquid silicone, potting compounds and thermal interface materials. Established in 2010 with a 40,000 m² production base, the company is an export-driven manufacturer with 70 to 80 percent of its business overseas, supplying B2B clients with OEM and ODM encapsulation and thermal management solutions.

Our range covers thermal grease from 1.0 to 6.0 W/m·K, thermally conductive potting compounds, silicone gels, mould making rubber and food grade silicone. Because the thermal grease and the potting compound for the same module come from one factory, your engineering team works with one technical contact and your purchasing team consolidates one supplier, one documentation set and one shipment schedule.

HN500 metal-filled thermal grease packaging drums

Send your cooler drawing, mounting pressure and target junction temperature and our application engineers will confirm the grade, the deposit pattern and the film thickness target, and arrange a 1 kg sample drum for your A/B test.

Tell us the module power, interface area and coolant or air temperature and we will reply with the expected interface contribution and a delivery schedule for Southeast Asia.